Latest ArticlesThis article introduces mainstream photovoltaic (PV) support products, with their performances and respective characteristics. For the steel of 800 MPa high-strength weather-resistant photovoltaic supports, the large number of alloying elements and their complex interactions cause significant performance fluctuations, which affect processing and application. To address this problem, this study proposes an approach using data processing technology to guide production and designs a digital production control platform. The platform uses machine learning algorithms to establish data acquisition and preprocessing, data analysis module, and process optimization module. By analyzing more than 2 000 sets of on-site production data and combining with the accuracy comparison results of five classic models, the weighted average method combining random forest (RF) and deep neural network (DNN) has been finally selected to construct the data analysis module for process optimization guidance. The comparative results show that digital production control technology significantly improves the performance stability of 800 MPa grade weathering steel. Among them, the process capability index of strength increases from inadequate levels (0.89 and 0.67) to excellent and satisfactory levels (1.70 and 1.42). The digital production control platform effectively resolves the stability control problem of multi-alloy designed products, and also provides technical methods and implementation pathways for digital empowerment of the traditional equipment manufacturing industry.
To reveal the impact mechanism of Ti element in Ti-bearing steel grades on the sintering of ladle filler sands, laboratory experiments were conducted to investigate the effect of different Ti contents on the sintering behaviors of silica-based, chromite-based and zircon-based filler sands. The results show that with the increase of Ti content in steel, the liquid phase generated in the sintered sands increases significantly under the impact of liquid steel. The components (e.g., SiO2 and MnO) in the liquid phase react with dissolved Ti in steel, leading to the rise of Ti2O3 content in the liquid phase. Ti in steel can lower the melting point of the liquid phase inside the sintered filler sands, and promote the formation of the liquid phase. Meanwhile, under the impact of Ti, zircon-based filler sands decompose into many fine zirconia particles, and a large number of pores are formed after the shrinkage of the sintered grains. The sintering degree of silica-based filler sands is the severest. Considering both the performance and cost, chromite-based filler sands are more suitable for Ti-bearing steel grades.
To investigate the feasibility of applying high-purity salt-lake magnesia with abundant reserves as a substitute for fused magnesite derived from magnesite in MgO-C bricks, the microstructure and phase assemblage of high-purity salt-lake magnesia prepared from salt-lake brine were analyzed. Meanwhile, two types of MgO-C bricks for steel ladle slag line were fabricated using high-purity salt-lake magnesia and fused magnesite from magnesite as raw materials respectively, with phenolic resin and graphite added as additives. According to national standards, the two brick samples were tested and compared in terms of bulk density, apparent porosity, cold compressive strength, hot modulus of rupture, phase assemblage and microstructure. Industrial comparative trials were further carried out on the slag-line working layer of ladles. The results show that high-purity salt-lake magnesia possesses a dense microstructure, with periclase as its dominant phase, featuring high magnesia content and low impurity levels. The MgO-C bricks prepared from high-purity salt-lake magnesia exhibited superior physicochemical properties compared with the brick produced from magnesite-based fused magnesia. Under steel ladle service conditions, the brick made from salt-lake magnesia could satisfactorily replace the counterpart fabricated from fused magnesite derived from magnesite.
In order to investigate the effect of slag length on the wear of the flue wall during the copper flash smelting process, a numerical analysis has been carried out using a two-fluid model. The results indicate that the wear area on the upstream side of the flue wall increases initially and then decreases as the slag length increases. When the slag length reaches 0.4 m, the wear degree reaches its maximum, with a wear area of 2 m in height and 0.6 m in width. It is found that reducing the slag length can prevent the high-intensity wall erosion which is caused by the high-speed flue flow. Additionally, when the slag length reaches 0.5 m, the wall surface can be protected by altering the flow pattern of the multi-phase flue flow. Furthermore, reducing the airflow rate can effectively weaken the erosion on the flue wall. When the slag length is 0.4 m, a reduction of 2 000 m3/h on the airflow rate from 22 103 m3/h to 12 103 m3/h can result in a corresponding reduction in erosion intensity of 4.8%, 10.5%, 5.6%, 13.2%, and 17.7%, respectively. When the slag length is 0.5 m, the wear intensity in local areas is found to increase as the airflow rate decreases. However, the general trend of reduced erosion with decreasing the airflow rate is consistent with that when the slag length is 0.4 m, and the wear intensity is lower when the slag length is larger.
The uniformity of gas exhaust among cells is a key factor affecting the environmental quality in the potroom. Measurement data from the 350 kA potline show that the total pressure drop in the branch pipes on the side toward which the main collection duct is biased toward generally higher than that on the opposite side. This study establishes a gas flow field model for the branch pipe system and the main collection duct. The computational results indicate that only when the flow area of the branch pipes on the biased side is 11.4% smaller than that on the opposite side can gas exhaust among cells be effectively balanced. This configuration increases the pressure drop of the main collection duct by 13.6% compared to a symmetrically arranged system. The discovery that the bias of the main collection duct inversely affects gas exhaust among cells enhances the aluminum industry's understanding of balanced gas exhaust and provides a theoretical basis for improving potroom environmental quality and thermal balance among cells.
4J29 alloy has been used as the research object, and samples with different Ce additions have been prepared by a vacuum induction furnace. The effects of Ce addition on the microstructure and corrosion resistance of the alloy have been systematically investigated by means of optical microscope, scanning electron microscope, potentiodynamic polarization curve and electrochemical impedance spectroscopy. The results show that Ce addition can significantly refine the alloy grains, straighten grain boundaries, and modify the original harmful inclusions into fine and well-rounded Ce-containing rare earth inclusions. The transformation path of inclusions is determined to Al2O3→CeAlO3→CeO2S→Ce2O3→CeO2. In 3.5%NaCl(mass fraction) solution, Ce can positively shift the corrosion potential and pitting potential, and reduce the corrosion current density. The corrosion resistance increases first and then decreases slightly with the increase of Ce addition. When the Ce addition is 0.013%, the inclusion refinement is the best, the passive film is the thickest and most compact, and the comprehensive corrosion resistance of the alloy is optimal.
By means of microstructure characterization and property testing, the uniformity of microstructure and properties of a 480 mm thick high-alloyed Al-Zn-Mg-Cu alloy flat ingot prepared by semi-continuous casting in industrial mass production has been investigated. Inductively coupled plasma optical emission spectrometry (ICP-OES) is adopted to detect the distribution of alloying element contents at different thickness positions of the ingot. Optical microscopy (OM), scanning electron microscopy (SEM), and other equipment are used to characterize the grain morphology, type, and content of second phases at various thickness locations. A microhardness tester and electrical conductivity tester are employed to measure the differences in mechanical and conductive properties of the ingot at different thickness positions. The results show that segregation of alloying elements including Zn, Mg, and Cu exists within the range of 100~150 mm from the surface along the thickness direction of the ingot. Four types of grain morphologies appear sequentially along the 8 mm section from the solidified shell layer to the center of the ingot, namely shell fine-grained zone, non-uniform columnar grain zone, equiaxed grain zone with few dendrites and compounds, and local zone with densely distributed dendrites and compounds. The near-surface region of the ingot exhibits a relatively small number of secondary dendrites; as extending from the surface towards the center along the thickness direction, the dendrite features become more prominent, and the grain size increases gradually. In addition, abundant large-sized non-equilibrium second phases are distributed at the 1/4 thickness position of the ingot. Affected by these coarse non-equilibrium precipitates, this position exhibits the lowest microhardness (HV) and highest electrical conductivity, which are 135.6 and 41.2 %IACS, respectively.